Analisis Pengaruh Perbandingan Komposisi dan Waktu terhadap Kekerasan Produk Hasil Percampuran High Density Polyethylene dan Karet SBR

The Effect of Composition and Time Comparison on Product Hardness Result from the Mixing of High Density Polyethylene and SBR Rubber

YUDA DWI RADIDTYA

THE EFFECT OF COMPOSITION AND TIME COMPARISON ON PRODUCT HARDNESS RESULTS FROM THE MIXING OF HIGH DENSITY POLYTHYLENE AND SBR RUBBER Plastic is a type of solid waste that is difficult to destroy and its volume continues to increase. This type of high density polyethylene plastic is easily recycled back into a variety of products a plastic recycling business. Durometer is an instrument that uses the working principle used to measure or test the hardness of rubber, a plastic. SBR (Styrene Butadiene Rubber) rubber is one of the best polymers that are widely produced and used in the world today. SBR rubber is a of synthetic rubber that is the most widely used, has good abrasion resistance and heat or heat generated is also low. The purpose of this study is to determine the composition that is suitable for making the product, to determine the amount of mixture ratio between high density polyethylene and SBR rubber, to investigate and analyze the effect of the time of the melting of high density polyethylene and SBR rubber. This research method uses factorial two way ANOVA and for an analysis of researching data using Minitab 17 software applications. The results of this study are the results of a comparison of 50% HDPE: 50% of SBR rubber produces the highest hardness value of 39.33 HD, while the lowest is in the ratio of 40% HDPE: 60% of SBR rubber produces a hardness value of 33.6 HD The conclusion of this research is that each time variation and comparison of the composition of materials have a significant effect on the value of product hardness.

© 2026 UPA Perpustakaan POLINEMAStatus LayananKebijakan PrivasiSyarat & Ketentuan

v2026.11.28.2 · c6ad4ed