Pengaruh Variasi Temperatur dan Holding Time pada Metode Fasa Ganda terhadap Kekuatan Tarik dan Kekerasan Baja Karbon Rendah ASTM A36 dengan Sambungan Butt Joint Las Mig
The Influence of Variations of Temperature and Holding Time in Dual Phase Method on Tensile Strength and Hardness of Low Carbon Steel ASTM A36 with Butt Joint Mig Welding
Low carbon steel is one of the materials widely used in industry because it has relatively affordable and easy welding process. But the weakness has a low value of tensile strength and hardness. Low carbon steel can be increased in value of tensile strength and hardness by using a dual phase method so that it can be used in situations that require higher tensile strength and hardness. To know the effect of temperature and holding time on the tensile strength and hardness of ASTM A36 with the dual phase method and compare with welding process. Variation of temperatur used 730°C with holding time of 5 minutes, temperature of 750°C with holding time of 10 minutes, temperature of 770°C with holding time of 15 minutes, 790°C with holding time of 20 minutes, and then temperature of 810°C with holding time of 30 minutes . The research concluded after experiencing welding, tensile strength of ASTM A36 steel has increased, the highest tensile strength 488.01 N / mm2 in the specimen by welding this due to the mixing of the material with the electrode at the time of melting in the welding process. The highest of hardness value was obtained at temperatur 730°C with a holding time of 5 minutes with Vickers of hardness value of 9.12. The suggestion for next research to use different temperature variations to find out the other temperature variations and can be made as a comparison also use other types of material to determine the strength of different materials and can be made as a comparison.