Pengaruh Sudut dan Temperatur Preheat Terhadap Kekuatan Corner Joint Baja SS400 Pada FCAW
The Effect Of Angle and Preheat Temperature On Strength Of Corner Joint Steel SS400 On FCAW
Technology is currently developing rapidly, especially in the manufacturing. In the manufacturing world there is a metal joining technique, namely welding technique. Welding is a metal joining process where the metal becomes one due to the heat of welding. In this study, the welding process used is Flux Core Arc Welding (FCAW). FCAW is a type of electric welding that mechanically adds a filler electrode into an electric arc formed between the tip of the filler electrode and the parent metal, and uses carbon CO2 as a shielding gas. The specimens were made by adjusting the welding angles of 35°, 45ᵒ and 55ᵒ and the preheat temperature variations of 80°C, 130°C, and 180°C. The purpose of this research was to determine the effect of preheat temperature and welding angle on fillet joints on SS400 Steel on FCAW. Based on the results of the research that has been done, the variation of the welding angle shows that the highest stress strain is located at the welding angle at 45° and the lowest stress strain is at the welding angle at 35°. And there is an influence on the interaction of the welding angle and preheat temperature on the strength of the corner joint in welding FCAW. The highest average strength value is found at 45° welding angle and 130°C preheat temperature of 584 N/mm².