Pembuatan Biodegradable Foam Menggunakan Pati Sagu Termodifikasi pada berbagai Variasi Konsentrasi Kitosan.
Producing Biodegradable Foam Using Modified Sago Starch in Various Variations of Chitosan Concentration.
DWI FIRDAUS MABRUR ROHMAN, ARI ISHLAHUDDIN
Biodegradable foam is an alternative packaging for styrofoam which uses the main raw material in the form of starch so that the packaging can be decomposed naturally. However, the biodegradable foam products produced still have low characteristics. This research is conducted to determine the effect of the addition of chitosan concentration on the characteristics of biodegradable foam properties produced from modified sago starch using acid-alcohol hydrolysis method. The type of acid used in acid hydrolysis is HCl and H2SO4. The concentrations of chitosan added in this study are varied from 0, 5, 10, 15, 20, 25, 30% w / w of starch. Biodegradable foam manufacturing is carried out by using the baking process method which begins with the mixing of ingredients other than modified sago starch, stirring until the mixture becomes homogeneous and expands, and baked in an oven at 125ºC. The analysis made on acid-alcohol modified starch is functional group analysis using FT-IR spectroscopy while the analysis of biodegradable foam are water absorption analysis, biodegradability analysis, density and tensile test. The result reveals that modification of acidalcohol on sago starch do not affect the functional group. The best mechanical properties of biodegradable foam in this study are obtained by using HClmodified sago starch and addition of chitosan by 20% w / w which have an absorption capacity of 4.95%, density of 0.6 g / m3, degradation ability of 25.12% and tensile strength of 1.27 MPa.