High Energy Milling Of Magnesium With Zeolite For Hydrogen Storage

Adhira Satria Pratama

Currently, there are many developments in renewable fuel sources to replace fossil fuels as the main fuel. Hydrogen fuel is one of the promising candidates to replace fossil fuels because it is environmentally friendly. However, storing hydrogen in a safe, efficient and economical way remains a challenge at present. Magnesium (Mg) has received great attention as a potential material for hydrogen storage due to its high gravimetric hydrogen storage capacity, disclosure, and low cost. However, it is compromised by high thermodynamic stability and low kinetics. Utilization of zeolite-based catalysts along with magnesium (Mg) for hydrogen storage provides a promising opportunity to overcome the challenges associated with slow kinetics and high desorption temperatures. High-energy milling is a promising technique for improving the hydrogen storage properties of materials, especially magnesium- and zeolite-based compounds. This paper explores the synergistic effect of high-energy milling on the performance of magnesiumand zeolite-based hydrogen storage. By applying a strong mechanical force to the material during grinding, the structure and properties of the material can be finely adjusted, thereby improving the kinetics and hydrogen absorption capacity. High-energy ball milling is used to mix Mg with 5A zeolite and Ni. Characterization of the crystal structure and morphological characteristics of the samples was carried out using X-ray diffraction (XRD). The crystal size decreases, and significant grain size refinement occurs. The size of the Mg+5A zeolite +Ni sample calculated from XRD data is in the range of 38.2-49.3 nm, while the Mg grain size before ball milling is 63.6-91.1 nm. The kinetic properties of absorption and desorption were also evaluated using pressure-compositiontemperature (PCT) equipment. The results showed that at a temperature of 330°C and pressure 2,5 MPa, the Mg+30wt.%5A zeolite+10wt.% Ni sample, with a milling speed of 45Hz and a milling time of 4 hours had absorption and desorption capacity of 2.55 wt.% and 2.53 wt.%, each in less than 20 minutes. The PCT isotherms were obtained at temperatures of 270°C, 300°C, 330°C, and the pressure is 10 bar. The reversible hydrogen storage capacity was about 2.6 wt.%. The equilibrium pressure plateau for absorption at temperatures of 270°C, 300°C, and 330°C is 0.113 MPa, 0.286 MPa, and 0.660 MPa, respectively. The plateau equilibrium pressures for desorption at 270°C, 300°C, and 330°C are 0.187 MPa, 0.164 MPa, and 0.184 MPa, respectively

© 2026 UPA Perpustakaan POLINEMAStatus LayananKebijakan PrivasiSyarat & Ketentuan

v2026.11.23.3 · f3541dc